Biophysical Properties, Antimicrobial Activity, and In Vitro Fibroblast Migration of Propolis-Loaded Electrospun Polycaprolactone Fibers

Document Type : Research Article

Authors

1 Department of Biophysics, Faculty of Biological Science, Tarbiat Modares University, 14115-154, Tehran, Iran

2 Biotechnology Research Center, Yazd Reproductive Sciences Institute, Shahid Sadoughi University of Medical Sciences, Yazd, Iran

3 School of Advanced Medical Technologies, Shahid Sadoughi University of Medical Sciences, Yazd, Iran

4 Department of Food Nanotechnology, Research Institute of Food Science and Technology (RIFST), Mashhad, Iran

5 Department of Nutrition, School of Allied Medical Sciences, Ahvaz Jundishapur University of Medical Sciences, Ahvaz, Iran

Abstract

Propolis, a resinous substance produced by honeybees, possesses potent antioxidant, antimicrobial, and regenerative properties, making it a promising bioactive agent for wound healing. Electrospun Polycaprolactone fibers containing 10% Propolis were prepared using a chloroform–methanol solvent system and compared with Propolis-free control fibers. The samples were characterized for morphology, thermal and mechanical properties, wettability, antimicrobial activity, in vitro wound healing using a fibroblast scratch assay, and molecular docking of pinobanksin with wound-healing-related proteins, followed by statistical analysis using an independent samples t-test. SEM images revealed a uniform fiber network with reduced pore size in Propolis-loaded samples, while WDX confirmed the loading of Propolis extract into the fibers. Propolis slightly increased the melting temperature from 61.6 °C to 63.8 °C. The water contact angle decreased from 113.2° to 64.4°, indicating increased surface wettability and decreased tensile strength from 1.98 MPa to 0.86 MPa. The fibers showed strong antibacterial activity against E. coli and Staphylococcus aureus with 99.5% reduction, antifungal activity against Mucor racemosus with 70% reduction, enhanced fibroblast migration with 84.97% wound closure, and strong pinobanksin binding to wound-related proteins such as 966C (−10.1 kcal/mol) and 4XCT (−9.5 kcal/mol). These results indicate that electrospun fibers containing Propolis can contribute to the development of wound dressings. However, in the scratch assay, electrospun fibers containing Propolis did not perform better than the control sample, a finding that warrants further investigation.

Keywords

Main Subjects